Mixing
Refer to the bag for how much water the plaster requires. Add the dry material to the water and mix with a concrete mixer for around ten minutes. With a power mixer or a drill paddle, around two to three minutes of mixing is sufficient. Let the plaster stand for around five minutes and mix it again for a short while. Find the correct consistency at this stage by gradually adding the rest of the water. We do not recommend adding all of the water right at the start. The finished plaster remains workable for around one hour.
Work instructions
Designed for thin-joint masonry in the temperature range -15°C...+5°C.
Follow the instructions of the designers and official regulations in masonry work.
National Building Code of Finland B5 and National Building Code of Finland B8, and RYL 2000 instructions.
Other points to note
Winter products will be available in the winter season, from 15 September to 1 March. At other times, the products must be ordered separately.
Storage and handling of waste
See the separate storage and disposal instructions https://www.fescon.fi/en/material-bank